BJS 150 Performances
Poly crystalline diamond
Quality : no visible nitrogen in PL at liquid nitrogen temperature
Growth speed : up to 20 µm/h depending on growth conditions
Uniformity : ± 5% on 2’’
Mono-crystalline diamond :
PNo visible nitrogen in PL at liquid nitrogen temperature
Nitrogen concentration measured by EPR : [NsO] < 1 ppb
FWHM of the diamond Raman line at 1332 cm-1 : 1.6 cm-1
No infrared absorption from 4000 – 10000 cm-1
Growth speed : up to 20 µm/h on growth